Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 36.55 MPa | 5301 psi | ASTM D790 |
Lucent Polymers CPP-330 Polypropylene, 30% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |