Polymer Property : Flexural Strength = 361 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 361 MPa
52400 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66
LNP* STAT-KON* REF42 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Strength 361 MPa

@Temperature -40.0 °C
52400 psi

@Temperature -40.0 °F
ASTM Test
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
Flexural Strength 361 MPa
52400 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 (Asia Pacific)
LNP* Stat-kon* REF42 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Fiber.