Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 0.2561 MPa | 37.14 psi | ASTM D790 |
Sekisui PIOCELAN LSP-40EB Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |