Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 25.9 MPa | 3750 psi | ASTM D790 |
Multibase Multi-Pro® 5012 C Natural Polypropylene Forms:PelletsProcessing Methods:Injection MoldingFeatures:Gloss, LowInformation provided by Multibase |