Mechanical Properties Metric English Comments
Flexural Strength 2.60 MPa
377 psi
1% Sec; ASTM D-790-92
Multibase Multi-Flex® TPE A 8502 EXCEL GREY
Heating aging the material 1000 hours at 125°C leads to a +7% change in the tensile strength, +4% change in elongation, and +12% change in tear strength. Ash is 16%. Multi-Flex TPE contains Krato..
Flexural Strength 2.60 MPa
377 psi
1% Sec; ASTM D-790-92
Multibase Multi-Flex® TPE A 8592 MEDIUM TAUPE
Heating aging the material 1000 hours at 125°C leads to a +7% change in the tensile strength, +4% change in elongation, and +12% change in tear strength. Ash is 16%. Multi-Flex TPE contains Krato..
Flexural Strength 2.60 MPa
377 psi
ASTM D790
Solvay Specialty Polymers Veradel® 3000RP Polyethersulfone (PESU)
Veradel® 3000RP hydroxyl-functionalized polyethersulfones (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersi..
Flexural Strength 2.60 MPa
377 psi
ASTM D790
Solvay Specialty Polymers Veradel® 3600RP Polyethersulfone (PESU)
Veradel® 3600RP hydroxyl-functionalized polyethersulfone (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersin..
Flexural Strength 2.60 MPa
377 psi
ASTM D790
Solvay Specialty Polymers Veradel® 3000RP Polyethersulfone (PESU)  (Unverified Data**)
Veradel® 3000RP hydroxyl-functionalized polyethersulfones (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersing..
Flexural Strength 2.60 MPa
377 psi
ASTM D790
Solvay Specialty Polymers Veradel® 3600RP Polyethersulfone (PESU)  (Unverified Data**)
Veradel® 3600RP hydroxyl-functionalized polyethersulfone (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersing ..