Mechanical Properties Metric English Comments
Flexural Strength 2.62 MPa
380 psi
ISO 178
Multibase TPSiV® 4000-80A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob..
Flexural Strength 2.62 MPa
380 psi
BCC Products MB 1100 Polyurethane Foam Modeling Board
MB 1100 is an Olive colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1100 is low density foam of approximately 10lbs/ft3 board. Easily cut using CNC machining equipment or ..