Mechanical Properties Metric English Comments
Flexural Strength 39.24 MPa
5691 psi
Shinil Chemical SHINSTAT PETG Electrostatic Control Polymer Sheet Grade
SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for ..
Flexural Strength 39.24 MPa
5691 psi
Shinil Chemical SHINSTAT PP Electrostatic Control Polymer Sheet Grade
SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for ..
Flexural Strength 39.24 MPa
5691 psi
Shinil Chemical SHINSTRA PA-66 Devlop Structural Polymer Window Strip
SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog..