Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 413 MPa | 59900 psi | ASTM D790 |
Quantum Composites LYTEX® 4181 55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4181 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance.. |
|||
Flexural Strength | 413 MPa | 59900 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RX04515H PA 66 LNP* Thermocomp* RX04515H is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 413 MPa | 59900 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UC006H PPA LNP THERMOCOMP* UC006H is a compound based on Polyphthalamide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |