Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 2960 MPa | 429000 psi | |
China Tungsten YG20C Tungsten Carbide for Dies and Wear Part Making For cold forging, punching pressing dies for standard components bearings and tools industries etc; and for punching dies for bullet heads and cartridges.Information provided by China Tungsten |