Polymer Property : Flexural Strength = 430 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 430 MPa
62400 psi
Lehmann & Voss LUVOCOM® 20-7847 Polyphthalamide, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Flexural Strength 430 MPa
62400 psi
ASTM D790
Mitsui Arlenâ„¢ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
Flexural Strength >= 430 MPa
>= 62400 psi
Limit of elasticity in Bending
CLAL-MSX SICLANIC S® TF Quenched Copper Alloy, precipitation treated
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Flexural Strength 430 MPa

@Temperature 23.0 °C
62400 psi

@Temperature 73.4 °F
Elisto THERMOSTAR® LC 610 Insulation Material
Pattern material. Insulation materials for mechanical engineering.Information provided by elisto
Flexural Strength 430 MPa
62400 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON RV00CES PA 66
LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Flexural Strength 430 MPa
62400 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66
LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Flexural Strength 430 MPa
62400 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Verton RV00CEU PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00CEU is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, UV Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Flexural Strength 430 MPa
62400 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON RV00CEXP PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00CE is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding.
Flexural Strength 430 MPa
62400 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON RX06424 PA 66
LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural