Polymer Property : Flexural Strength = 46856 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 323.06 MPa
46856 psi
Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D790
Fibre Glast Saf-T-Poxy 2410 / 2183 Epoxy  (discontinued **)
Information provided by Fibre Glast Developments Corporation.