Mechanical Properties Metric English Comments
Flexural Strength 472 MPa
68500 psi
Rigidty. Elastic bending fatigue, Longitudinal
CLAL-MSX NICLAFOR® 1000 TDX Quenched/Cold Rolled, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..