Polymer Property : Flexural Strength = 4826 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 4826 MPa
700000 psi
Hardening Temperature- 1190°C, Tempering Temperature- 550°C
Crucible Steel CPM® Rex® 45® (HS) High Speed Steel
CPM Rex 45 is an 8% cobalt modification of M3 high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It has red hardness comparable to that of M42 but offers abrasion resistance ev..