Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 345 MPa | 50000 psi | ASTM D790 |
Oxford Polymers Oxnilon 6-50GF 50% Glass Fiber Filled Nylon 6 for Injection Molding 50% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Strength | 345 MPa | 50000 psi | Transverse Rupture |
Pacific Sintered Materials F-241-S Iron Powdered Metal Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-15All information provided by Pacific Sintered Metals. |
|||
Flexural Strength | 345 MPa | 50000 psi | |
Pyrotek TS-103 Thermoset Electrical Insulation Product (Nema Grade: G-3) Glass reinforcement, Phenolic resin, Natural color. Good heat resistance. Excellent mechanical and machining properties.ApplicationsSuperstructure support pads Bus bar insulators Pot cradle insula.. |
|||
Flexural Strength | 345 MPa | 50000 psi | |
Pyrotek TS-206 Thermoset Electrical Insulation Product Glass reinforcement, Polyester resin, Dark Red color. High compressive and flexural strength.Information provided by Pyrotek. |
|||
Flexural Strength | 345 MPa | 50000 psi | Transverse Rupture |
PSM Industries Pacific Sintered Metals Copper Iron FC-208-N Powdered Metal Excellent for self-lubricating parts and heavy duty bearings. Equivalent MPIF Specification: FC-2000-K40Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Flexural Strength | 345 MPa | 50000 psi | Transverse Rupture |
PSM Industries Pacific Sintered Metals Iron F-241-S Powdered Metal Low stressed mechanical components, Soft magnetic applications Equivalent MPIF Specification: F-0000-15Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Flexural Strength | 345 MPa | 50000 psi | |
Lehmann & Voss LUVOCOM® 1105-8529 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Strength | 345 MPa | 50000 psi | |
Lehmann & Voss LUVOCOM® 1-7791 Polyamide 66, with carbon fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Flexural Strength | 345 MPa | 50000 psi | |
Lehmann & Voss LUVOCOM® 19/CF/30 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Strength | 345 MPa | 50000 psi | |
Lehmann & Voss LUVOCOM® 1105/XCF/15 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Strength | 345 MPa | 50000 psi | ASTM D790 |
Techmer ES Electrablend® PA6/6 CF30 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf.. |
|||
Flexural Strength | 345 MPa | 50000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 345 MPa | 50000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF60 HS L 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati.. |
|||
Flexural Strength | 345 MPa | 50000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF60 HS L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackProcessing Method: In.. |
|||
Flexural Strength | 345 MPa | 50000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF60 HS UV BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Flexural Strength | 345 MPa | 50000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF60 L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackInformation provided by TP Com.. |
|||
Flexural Strength | 345 MPa | 50000 psi | At Rupture; ASTM D790 |
Sumitomo Bakelite North America EM 7302 Hardware Grade Epoxy Long fiberglass reinforced epoxy molding compound which features high strength and toughness for structural components. This compound is designed for applications requiring Mil-M-46069 certificatio.. |
|||
Flexural Strength | 345 MPa | 50000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PX12419 PA 6 LNP* THERMOCOMP* PX12419 is a compound based on Nylon 6 containing Carbon Fiber. Added features of this grade include: Electrically Conductive. |
|||
Flexural Strength | 345 MPa | 50000 psi | |
Cosmic Plastics CP7311 Epoxy Molding Compound Data provided by the manufacturer. |
|||
Flexural Strength | 345 MPa | 50000 psi | ISO 178-93 |
Wellman Wellamid® GF1750-N2 50% Glass Fiber Reinforced Nylon 6 Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Flexural Strength | 345 MPa | 50000 psi | at max force; ISO 178 |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |