Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 35.2 MPa | 5100 psi | ASTM D790 |
Techmer ES HiFill FR® HDPE FR-2 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 35.2 MPa | 5100 psi | ASTM D790 |
Techmer ES HiFill FR® HDPE FR-HB Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 35.2 MPa | 5100 psi | ASTM D790 |
Quadrant EPP Sanalite® PP, Homopolymer Polypropylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet) |