Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 352 MPa | 51000 psi | ASTM D790 |
Techmer ES HiFill® PA4/6 CF40 HS 40% Carbon Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Flexural Strength | 352 MPa | 51000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF43 L BK 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackProcessing Method: Injection Mol.. |
|||
Flexural Strength | 352 MPa | 51000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF44 HS L 44% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 44% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabilized TPCI# 95.. |
|||
Flexural Strength | 352 MPa | 51000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF44 HS X 44% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 44% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabilized TPCI# 95.. |
|||
Flexural Strength | 352 MPa | 51000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 LGF60 HS L BK 12 mm Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass FiberAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Good MoldabilityAppearance: BlackProce.. |
|||
Flexural Strength | 352 MPa | 51000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF70 HS L BK 70% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 70% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Flexural Strength | 352 MPa | 51000 psi | ASTM D790 |
PolyOne Edgetek® AM-40CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |