Polymer Property : Flexural Strength = 5129 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 5129 MPa
743900 psi
Hardening Temperature- 1165°C, Tempering Temperature- 565°C
Crucible Steel CPM® Rex M4 HC(HS) Tool Steel
CPM REX M4 HC(HS) is a high vanadium special purpose high speed steel exhibiting better wear resistance and toughness than M2 or M3 in cold work punches, die inserts and cutting applications involvi..