Polymer Property : Flexural Strength = 5155 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 35.54 MPa
5155 psi
ASTM D790
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene
DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid..
Flexural Strength 35.54 MPa
5155 psi
ASTM D790
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene
DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid..
Flexural Strength 35.54 MPa
5155 psi
ASTM D790
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene
DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid..
Flexural Strength 35.54 MPa
5155 psi
ASTM D790
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene
DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid..
Flexural Strength 35.54 MPa
5155 psi
ASTM D790
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene
DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid..
Flexural Strength 35.54 MPa
5155 psi
ASTM D790
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene
DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid..