Polymer Property : Flexural Strength = 52.1 MPa
Polymer Property :
Flexural Strength =
52.1 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Strength
52.1
MPa
7550
psi
ASTM D 790
Styrolution PS 7800 HIPS
Extremely high surface glossGood processabilityUL Classification 94 HBInformation provided by Styrolution