Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 53.4 MPa | 7750 psi | |
Poco Graphite PYROGRAPH Ion Implant Grade Graphite Pyrograph is pyrolytically infiltrated graphite. POCO's proprietary process infiltrates the base material to a minimum depth of 0.1 inch throughout the entire surface of the component. This process .. |