Polymer Property : Flexural Strength = 55561 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 383.08 MPa
55561 psi
Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D790
Fibre Glast ProSet 125R / 229H Epoxy  (discontinued **)
Information provided by Fibre Glast Developments Corporation.