Flexural Strength 59.98 MPa
8699 psi
Abatron AboCast 8-8/Abocure 8-8 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 1 lb. (2.2 kg): 135 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F)...