Polymer Property : Flexural Strength = 60000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 414 MPa
60000 psi
ASTM D-790
PlastiComp Complet® LCF40 - PA66 Nylon 66, 40% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Flexural Strength 414 MPa
60000 psi
ASTM D790
PlastiComp Complet® LCF40-PA66 40% Long Carbon Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Flexural Strength 414 MPa
60000 psi
ASTM D790
LNP Thermocomp® UC-1006 Polyphthalamide, Carbon Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Flexural Strength 414 MPa
60000 psi
ASTM D790
Techmer ES HiFill® PEEK CF40 HF 40% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc.
Flexural Strength 414 MPa
60000 psi
MOR; ASTM-F417
CoorsTek PlasmaPure-UC™ 99.9% Alumina
Flexural Strength 414 MPa
60000 psi
Du-Co Ceramics DC-265-L-6 Alumina, 96% Al2O3
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Flexural Strength 414 MPa
60000 psi
IPC TM-650 2.4.4
Arlon 37N Polyimide Low-Flow
37N is a polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow is requir..
Flexural Strength 414 MPa
60000 psi
IPC TM-650 2.4.4
Arlon 38N High Performance Polyimide Low-Flow
38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow..
Flexural Strength 414 MPa
60000 psi
Aremco AREMCOLOX™ 502-1900-MTTZ Dense MgO Partially Stabilized Zirconium Oxide
This grade offers a high level of fracture toughness for a zirconia material. Features include excellent fracture, corrosion, thermal shock, and wear resistance. Used for pump parts, valve component..
Flexural Strength 414 MPa
60000 psi
20 x 40 mm
CeramTec 433 Alumina, 99.9%
433 (99.9%) is an alumina that exhibits high hardness. Its fine, equiaxial microstructure provides excellent sliding and abrasive wear resistance. This material is ideal for corrosive conditions. A ..