Mechanical Properties Metric English Comments
Flexural Strength 41.38 MPa
6002 psi
ASTM D790
Lucent Polymers CPP-220 Polypropylene, 20% Calcium Carbonate Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Strength 41.38 MPa
6002 psi
ASTM D790
Lucent Polymers TPP-310 Polypropylene, 10% Talc Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Strength 41.38 MPa
6002 psi
ASTM D790
Lucent Polymers PPH-110 Polypropylene, Homopolymer
Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.