Polymer Property : Flexural Strength = 62.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 62.8 MPa

@Thickness 3.20 mm
9110 psi

@Thickness 0.126 in
ASTM D790
LG Chemical LUMILOY GN1006F Injection Molding FR mPPO
Uses include electric/electronic parts.
Flexural Strength 62.8 MPa
9110 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® CM-0140UV ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Flexural Strength 62.8 MPa
9110 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® HF-0690M ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Flexural Strength 62.8 MPa
9110 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® PT-0180 ABS, Unreinforced Painting Grade
Information provided by Samsung Cheil Industries.
Flexural Strength 62.8 MPa
9110 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® SR-0310FM ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Flexural Strength 62.8 MPa
9110 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® SR-0315 V ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Flexural Strength 62.8 MPa
9110 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® SR-0320BM ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Flexural Strength 62.8 MPa
9110 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Flexural Strength 62.8 MPa
9110 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® CM-0140UV ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Flexural Strength 62.8 MPa
9110 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® HF-0690M ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Flexural Strength 62.8 MPa
9110 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® PT-0180 ABS, Unreinforced Painting Grade
Information provided by Samsung Cheil Industries.
Flexural Strength 62.8 MPa
9110 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® SR-0310FM ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Flexural Strength 62.8 MPa
9110 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® SR-0315 V ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Flexural Strength 62.8 MPa
9110 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® SR-0320BM ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Flexural Strength 62.8 MPa
9110 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Flexural Strength 62.8 MPa

@Thickness 3.20 mm
9110 psi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SP 6456 High Heat Polystyrene
Characteristics High heat resistance & strength Very good flow properties Available in any dark colorsProcessing Injection moldingApplications Instrument enclosures TV components Electrical encl..