Mechanical Properties Metric English Comments
Flexural Strength 621 MPa
90000 psi
Transverse Rupture
Pacific Sintered Materials FCC-216-P High Carbon Copper Steel Powdered Metal
High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI..
Flexural Strength 621 MPa
90000 psi
Transverse Rupture
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-216-P Powdered Metal
High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP..
Flexural Strength 621 MPa
90100 psi
ASTM D229
Glastic Laminates/Shapes Glass-Reinforced Polyester Topsticks
Data provided by Glastic Corporation.Pultruded with continuous glass fibers, available in many sizes. Used for motor stators.