Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 4377 MPa | 634800 psi | Hardening Temperature- 1120°C, Tempering Temperature- 550°C |
Crucible Steel CPM® 10V® (AISI A11) Tool Steel CPM 10V was the first in the family of high vanadium tool steels made by the Crucible Particle Metallurgy process. Crucible engineers optimized the vanadium content to provide superior wear resistan.. |