Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 65.15 MPa | 9449 psi | |
Abatron AboCast 8-5/Abocure 8-5 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/80.5 ratio (pbw); Gel time, 100 g (3.5 oz.): 300 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, a.. |