Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 45.2 MPa | 6560 psi | s.d. 1.3 MPa, specimen 2.48 cm wide (s.d. 0.01 cm), 0.22 cm thick (s.d.02 cm), 3.8 cm span (s.d. 0 cm). Test conditions: Humidity 50%, Temp. 23°C. |
Schmelzer Industries Pearlveil 110-7 Fiberglass Veil Economical alternative for flat or shallow applications. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. Data provided by the manufacturer, Schmelz.. |