Polymer Property : Flexural Strength = 660 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 4.55 MPa
660 psi
Saint-Gobain Rulon® DC7035 Bearing/Seal PTFE
Offers electrical conductivity in a low wear, self lubricating bearing material. This material is ideal in applications where static dissipation is needed. DC7035 is often used as a static bleed mec..