Mechanical Properties Metric English Comments
Flexural Strength 68.7 MPa
9960 psi
chs 0.05 in/min; ASTM D790
Diamond Polymers Centrex® 814 General Purpose Injection Molding Grade
Centrex 814 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and processing perfor..