Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D-790 |
Plaskolite Optix® CA - 927 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D-790 |
Plaskolite Optix® CP - 927 GHF High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Niche Polymer PPHM6BK Homopolymer PP Information provided by Niche Polymer |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Polymer Resources PPX-GP4-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Fiberfil® PP-60/TC/20 Polypropylene Homopolymer, 20% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Techmer ES HiFill® PA6 1030 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D 790 |
Styrolution Zylar 650 MBS Zylar® 650 is an impact modified styrene acrylic copolymer that provides a balance of clarity and toughness, with outstanding strength and rigidity. Zylar 650 also has superior processing charact.. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Teknor Apex Chemlon® 109 Nylon 66, Impact Grade Notes: High-Impact; Exceptional impact strength, especially at low temperatures; FMVSS Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Techmer ES HiFill® PA6 0254 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Techmer ES HiFill® PA6 0425 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Techmer ES HiFill® PA6 0445 A Availability: North AmericaForms: PelletsFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Techmer ES HiFill® POM 0212B Acetal Availability: North AmericaForms: PelletsFeatures: Copolymer and High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Techmer ES Luriblend® HDPE TL10 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Chase Plastics CP Pryme® PE-200-HD8M General Purpose High Density Polyethylene Information provided by Chase Plastics. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Ecomass® 1066ZD96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Technical Polymers |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Ecomass® 1080ZD94 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided by Techn.. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Ensinger Tecapeek® XP-104 Compression Molded PEEK Compound, with 7% Molybdenum Disulfide, 3% PTFE and 25% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Asahi Kasei Thermofil P-20TC-5103 20% Talc Reinforced, Lubricated, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Asahi Kasei Thermofil P-40MI-0600 40% Mica Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Asahi Kasei Thermofil P6-30MI-0533 30% Mica Reinforced, Flame Retardant, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 48.3 MPa | 7000 psi | ASTM D-790 |
Plaskolite West Optix® CP - 927 GHF High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Flexural Strength | 48.3 MPa | 7000 psi | at 0.05 in/min; ASTM D790 |
M. Holland Company IS300 Polystyrene, High Impact
(discontinued **) Uses: Audio Tapes, Household Goods, ToysApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by M. Holland. |