Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 72.9 - 75.7 MPa | 10600 - 11000 psi | ASTM D790M |
DSM Somos® ProtoCast™ AF 19122 Antimony-free Liquid Photopolymer Product DescriptionDSM Somos® ProtoCast™ AF 19122 is an antimony-free liquid photopolymer specifically formulated for producing investment casting patterns.ApplicationsIdeal for use in foundry app.. |