Mechanical Properties Metric English Comments
Flexural Strength 76.46 MPa
11090 psi
ASTM D-790
Axiall 3121 Rigid PVC, Extrusion
Georgia Gulf 3121 is an exterior grade powder compound formulated for processing applications requiring high production output rate. Having excellent weatherability and impact strength, 3121 is sui..