Polymer Property : Flexural Strength = 769000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 5300 MPa
769000 psi
(Fracture) @62HRC, Tempering: 3 x 1 h at 1040°F; Four-point bend
Bohler-Uddeholm UDDEHOLM VANADIS 23 (AISI M3:2) Hot Work Tool Steel
Chromium-molybdenum-tungsten-vanadium alloyed PM steelVanadis 23 is a high speed powder metallurgical steel, recommended for low temperature die casting applications and warm forging applications wh..