Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 5.52 - 5.53 MPa | 801 - 802 psi | |
FiberNide Nickel Aluminide Foam Atomic 22% Aluminum Description: This Nickel aluminide foam has excellent high temperature strength, oxidation resistance, and conductivity. This unique combination of properties makes this foam particularly suitable f.. |