Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 81.8 - 83.8 MPa | 11900 - 12200 psi | ASTM D790M |
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |