Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 82.4 MPa | 12000 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® CF-1030 PC, Unreinforced High Impact Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 82.4 MPa | 12000 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HN-1064 PC, Unreinforced FR PC material that is applied to other resin for mobile phone chargersInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 82.4 MPa | 12000 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HN-1064 PC, Unreinforced FR PC material that is applied to other resin for mobile phone chargersInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 82.4 MPa | 12000 psi | ASTM D790 |
Saint-Gobain Meldin® 3110 Thermoplastic Bearing Material 3110 has a very low coefficient of friction and is particularly well suited for use with soft mating surface materials such as aluminum and soft stainless steel. Meldin® 3100 materials have exce.. |
|||
Flexural Strength | 82.4 MPa | 12000 psi | chs 0.05 in/min; 5% strain; ASTM D790 |
Diamond Polymers PC 1035L Impact Modified, Polycarbonate, Injection Molding Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 82.4 MPa | 12000 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® CF-1030 PC, Unreinforced High Impact Information provided by Samsung Cheil Industries. |