Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 54.5 - 57.9 MPa | 7900 - 8400 psi | |
Ceradyne Thermo-Sil® UHS Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |