Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 849.4 MPa | 123200 psi | Prepreg, Warp Direction, RT, Dry, Normalized to 60% fiber volume fraction; ASTM D7264 |
Renegade Materials Corporation RM-5001 Cyanate Ester Prepreg, 6781 S2 Glass Fabric RM-5001 cyanate ester is a very low outgassing, toughened, high performance prepreg. Straightforward 350°F Cure Designed for the unique requirements of satellite and missile structuresLow shrinka.. |