Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 0.600 MPa | 87.0 psi | Parallel to thickness |
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Flexural Strength | 0.600 MPa | 87.0 psi | |
Lushan 2% WR-2 Wood Plastic Composites Compatibilizer Compatibilizer/coupling agent Lushan series for wood plastic composites is a maleic anhydride grafted polyolefins, applied in PE, PVC, wood powder, and bamboo powder and wood fiber composite materia.. |
|||
Flexural Strength | 0.600 MPa | 87.0 psi | Parallel to thickness |
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |