Polymer Property : Flexural Strength = 87.22 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 87.22 MPa
12650 psi
ASTM D790
Owens Corning Glass Fiber Reinforced Polyester BMC (Injection), 22 wt.% glass
Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u..