Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 88.29 MPa | 12810 psi | ASTM D790 |
E-Polymers TEKALOY® S630XB Heat Resistance, Weatherability PC/PBT Alloy PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistan.. |
|||
Flexural Strength | 88.29 MPa | 12810 psi | ASTM D790 |
E-Polymers TEKAMID® H14HR High Toughness Heat Resistance PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |
|||
Flexural Strength | 88.29 MPa | 12810 psi | ASTM D790 |