Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | >= 610 MPa | >= 88500 psi | cold bending |
China-Yixing Longly Refractories ZTA (10%ZrO2) Zirconia Toughened Alumina Composite Ceramic LONGLY's Zirconia Toughened Alumina ceramics (hereafter referred as composite ceramic, ZTA) is white, corrosion resistance, good chemical stability. As well all know that alumina is hard, while zir.. |
|||
Flexural Strength | 610 MPa | 88500 psi | |
Acerde Silicon Carbide Silicon Carbide key properties: High oxidation resistance, High hardness, Resistive to thermal stress, High thermal conductivity, Low thermal expansion, High elastic modulus, Superior chemical inert.. |
|||
Flexural Strength | 610 MPa | 88500 psi | |
Acerde Tungsten Tungsten key properties: Very high density, High oxidation resistance, Highest melting point of all metals, Lowest vapor pressure of all metals, Highest elasticity modulus of the all metals, Hardest.. |