Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 61.3 MPa | 8890 psi | ASTM D-790 |
Plaskolite Optix® CA - 1000 E High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Flexural Strength | 61.3 MPa | 8890 psi | ASTM D-790 |
Plaskolite Optix® CA - 1000 E-2 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Flexural Strength | 61.3 MPa | 8890 psi | ASTM D-790 |
Plaskolite Optix® CP - 1000 E High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Flexural Strength | 61.3 MPa | 8890 psi | ASTM D-790 |
Plaskolite West Optix® CP - 1000 E High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Flexural Strength | 61.3 MPa | 8890 psi | ASTM D-790 |
Plaskolite West Optix® CA - 1000 E High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Flexural Strength | 61.3 MPa | 8890 psi | ASTM D-790 |
Plaskolite West Optix® CA - 1000 E-2 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |