Polymer Property : Flexural Strength = 90.976 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 90.976 MPa
13195 psi
ASTM D790
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene
DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman.
Flexural Strength 90.976 MPa
13195 psi
ASTM D790
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene
DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman.
Flexural Strength 90.976 MPa
13195 psi
ASTM D790
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene
DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman.
Flexural Strength 90.976 MPa
13195 psi
ASTM D790
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene
DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman.
Flexural Strength 90.976 MPa
13195 psi
ASTM D790
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene
DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman.
Flexural Strength 90.976 MPa
13195 psi
ASTM D790
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene
DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman.