Mechanical Properties Metric English Comments
Flexural Strength 91.0 - 92.0 MPa
13200 - 13300 psi
ASTM D790
3D Systems Accura® accuGen™ HC and Ar Plastic for the SLA® 250 System
Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® 250 system.Typical ApplicationsMulti-purpose modelsRTV mold patternsForm/Fit/..