Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 634 MPa | 92000 psi | Rigidty. Elastic bending fatigue, Transverse |
CLAL-MSX NICLAFOR® 1000 TF Quenched/Precipitation Heat Treated, Rolled Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Flexural Strength | 634 MPa @Temperature 23.0 °C |
92000 psi @Temperature 73.4 °F |
|
Ceradyne CeraTrex™ 146-3E Silicon Carbide Features:high puritycorrosion resistancewear resistancetailored electrical properties Applications:semiconductor componentssputtering targetsballistic armorwear componentsInformation provided by Cer.. |