Polymer Property : Flexural Strength = 93.941 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 93.941 MPa
13625 psi
ASTM D790
PolyOne Stat-Tech™ PF-NX-062100-2 Polysulfone  (discontinued **)
Description/Features:Electrically ConductiveESD ProtectionInformation provided by PolyOne Corporation.