Flexural Strength 92.8 - 97.0 MPa
13500 - 14100 psi
ASTM D790
3D Systems Accura® 40 Plastic for SLA® Systems
40 Accura "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsHigh temperature testing:Automotive "under-the-hood" partsIntake manifoldsLighting components a..